Udimet 700 Alloy

Alloy name: Udimet 700
Diagram No.: 1019
Type of diagram: TTO
Chemical composition in weight %: 15.0% Cr, 0.15% Fe, 19.0% Co, 5.15% Mo, 3.4% Ti, 4.45% Al, 0.10% Si, O.l% Mn, 0.O28% B, 0.06% C, balance is Ni
Alloy group: Nickel-based alloys
Note: 700: Time-tempnture-oxidation diagram. Isoreactivit plots for constant amount of subscale damage. Note: complete reversal of behavior at 1040 C (1900 F) and absence of internal oxidation at this temperature. Treatment: 0.5-in. diam rod, solution annealed at 1177 C (2150 F) for 4 h, aged at 1080 C (1975 F) for 4 h + at 845 C (1550 F) for 24 h and at 870 C (1600 F) for 16 h.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.






Copyright © 2019 by Steel Data. All Rights Reserved.