Ni–12Co–2.5Cr–9W–6.4Re–6Al–5.5Ta–0.15Hf Alloy

Alloy name: Ni–12Co–2.5Cr–9W–6.4Re–6Al–5.5Ta–0.15Hf
Diagram No.: 1047
Type of diagram: TTT
Chemical composition in weight %: Ni–12Co–2.5Cr–9W–6.4Re–6Al–5.5Ta–0.15Hf
Alloy group: Nickel-based alloys
Note: Time–temperature-transformation (TTT) diagrams for the formation of TCP phases in two single-crystal superalloys, one with and the other without Ru-doping – the base composition being Ni–12Co–2.5Cr–9W–6.4Re–6Al–5.5Ta–0.15Hf (wt%). (Courtesy of An-Chou Yeh.)
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.








Copyright © 2019 by Steel Data. All Rights Reserved.