Incoloy 909 Alloy

Alloy name: Incoloy 909
Diagram No.: 1049
Type of diagram: TTT
Chemical composition in weight %: 42.1% Fe, 38.3% Ni, 12.9% Co, 4.70% Nb, 1.58% Ti, 0.35% Si, 0.04% Al, 0.01% C, 0.01% Cr
Alloy group: Iron-based alloys
Note: Isothermal aging after 1038 C/1h anneal. Figure, the TTT diagram for solution annealed alloy 909, shows the precipitation C-curves for the intragranular Gamma’, Eta”, Eta phases and the grain boundary (noted as G.B.) phases of the Laves and Eta types. G-phase silicides (A16B6Si7) form in the Laves region after prolonged exposures (>lOO hours). Minor phases present, but not shown, include (Nb,Ti)(C,N), TiN and Ti2C4S2.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.





Copyright © 2019 by Steel Data. All Rights Reserved.