718 Alloy

Alloy name: 718
Diagram No.: 1055
Type of diagram: TTT
Chemical composition in weight %: 50.00-55.00% Ni, 17.00-21.00% Cr, 4.75-5.50% Cb, 2.80-3.30% Mo, 0.20-0.80% Al, 0.65-1.15% Ti, max. 0.35% Mn, max. 0.35% Si, max. 0.006% B, max. 0.08% C, max. 0.15% S, Mg residual, balance is Fe
Alloy group: Nickel-based alloys
Note: Time-temperature-transformation diagram for alloy 718. Note that the material was solution-annealed at 2100 F (1149 C) for 1 hour and water-quenched.
A time-temperature-transformation diagram (T-T-T) for alloy 718 is shown in Figure. The T-T-T diagram shows a number of phases that precipitate in alloy 718 base metal: gamma prime, CbC, MeC, delta phase (Ni3Cb), and laves phase. All of these phases go into solution around 1950 F (1065 C). Because the grain-boundary phases are going into solution and are therefore no longer pinning the boundaries, grain growth occurs at temperatures above about 1900 F (1040 C).
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.


Copyright © 2019 by Steel Data. All Rights Reserved.