A625 Alloy

Alloy name: A625
Diagram No.: 1075
Type of diagram: TTT
Chemical composition in weight %: 20.5-22.5% Cr, 4.0-5.0% Fe, 8.1-8.9% Mo, 3.4-3.7% Nb+Ta, 0.01-0.40% C, 0.02-0.10% Mn, 0.05-0.10% Si, 0.02-0.04% Al, 0.1-0.25% Ti, balance is Ni
Alloy group: Nickel-based alloys
Note: Thermal exposures also can markedly change the microstructures of weld metal or castings. Even if care is taken to avoid Laves phase in the ascast structure, the enrichment in Nb in the interdendritic regions will lead to accelerated precipitation reactions upon heating. The Delta often could be seen to be localized in the interdendritic regions of the weld structure. Figure shows the effects of various thermal treatments on the appearance of Delta in this material, versus the T-T-T curve for Delta in wrought material. In this particular weld the time for Delta formation was reduced by a factor of about 50 versus the wrought material.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.