718 Alloy

Alloy name: 718
Diagram No.: 1081
Type of diagram: TTT
Chemical composition in weight %: 53.46% Ni, 18.65% Cr, 3.06% Mo, 5.08% Nb, 0.99% Ti, 0.72% Al, 0.035% C
Alloy group: Nickel-based alloys
Note: TTT Diagram of Alloy 718.
The TTT diagram of alloy 718 is given in Figure [8]. The precipitation reaction of interest in this work were: the equilibrium phase, Delat-Ni3Nb and the coherent precipitates, Gamma” and Gamma’. As seen in Figure, the ratio of precipitate hardening elements, Ti + Al/Nb, may affect the amount and solvus of coherent precipitates. New DTA approach suggested in this work offers an effective and efficient method to characterize this alloying effect.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.




Copyright © 2019 by Steel Data. All Rights Reserved.