718 Alloy

Alloy name: 718
Diagram No.: 1090
Type of diagram: TTT
Chemical composition in weight %: 52% Ni, 19% Fe, 19% Cr, 5.3% Nb, 3.1% Mo, 0.95% Ti, 0.55% Al
Alloy group: Nickel-based alloys
Note: El” diagram for alloy 718 from Basile and Radavich [9].
Reference: N. Saunders, M. Fahrmann and C. J. Small, THE APPLICATION OF CALPHAD CALCULATIONS TO NI-SUPERALLOYS, Superalloys 2000, Edited by T.M. Pollock, R.D. Kissinger, R.R. Bowman, K.A. Green, M. McLean, S. Olson, and J.J. Schirm, TMS (The Minerals, Metals &Materials Society), 2000, pp. 803-811.
Reference [9]: A. 0 Basile and J. F. Radavich ‘A Current ‘ITT Diagram for Wrought Alloy 718”, Superalloy 718,625 & Various Derivatives, ed. E. A Loria, (Warrendale, PATMS, 1991), p. 325.

Transformation Diagram


Click the image to enlarge the diagram.

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.