X-750 Alloy

Alloy name: X-750
Diagram No.: 1099
Type of diagram: TTT
Chemical composition in weight %: 72.0% Ni, 7.6% Fe, 15.4% Cr, 0.9% Al, 2.5% Ti, 0.9% Nb, 0.1% Si, 0.004% C
Alloy group: Nickel-based alloys
Note: Time-Temperature-Transformation Diagram for Alloy X-750 (12).
The time-temperature-transformation (TTT) diagram for the alloy was developed by A. A. Hesse in the late 1970s and is presented in Figure (13). Included in this study was a determination of the precipitated phases found during the course of the development of the TTT diagram. These phases are listed in Table. A. A. Hesse reported the MC carbides existed both in the grain boundaries and in the matrix. The M23C6 was only present in the grain boundaries. Electrolytic extractions indicated the maximum amount of precipitated carbides to be 0.2 to 0.3 weight percent and the amount of Gamma’ to be about 14 weight percent. The Eta phase occurs as thin plates, generally intraganularly.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.