ALLVAC 718PLUS Alloy

Alloy name: ALLVAC 718PLUS
Diagram No.: 1101
Type of diagram: TTT
Chemical composition in weight %: 0.025% C, 18.0% Cr, 2.70% Mo, 1.0% W, 9.0% Co, 10.0% Fe, 5.40% Nb, 0.70% Ti, 1.45% Al, 0.007% P, 0.004% B
Alloy group: Nickel-based alloys
Note: TTT Curves of Delta Phase Precipitation of Annealed Alloy 718Plus. Determined by Modeling (Solid Line) and Experiment (Dashed Line).
The TTT curve of Delta phase precipitation obtained by modeling and by experiment on super-solvus (1038C) treated alloy [10] is shown in Figure. It seems that Delata phase precipitation at grain boundaries is faster than the modeling prediction, but precipitation at other locations is sluggish. Since Delta phase precipitation temperature coincides with typical solution temperature in this alloy, it would be very interesting to study the Delta phase formation of hot worked material during solution treatment.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.



Copyright © 2019 by Steel Data. All Rights Reserved.