Rene 88 DT Alloy

Alloy name: Rene 88 DT
Diagram No.: 1105
Type of diagram: TTT
Chemical composition in weight %: 13% Co, 16% Cr, 4% Mo, 4% W, 2.1% Al, 3.7% Ti, 0.7% Nb, 0.03% C, 0.015% B, balance is Ni
Alloy group: Nickel-based alloys
Note: Schematic summary of phase reactions in Rene 88 DT. Prolonged exposure produces the growth of both the secondary and the tertiary forms of Gamma’ and the formation of grain boundary Gamma’ films. Ultimately, at exposure conditions equivalent to LM = 29 the tertiary Gamma’ that formed on aging dissolves. Continued exposure produces grain boundary M3B2 and M23C6 and, after prolonged exposure at 76O C, Mu phase appears. Full points were stressed exposures.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.





Copyright © 2019 by Steel Data. All Rights Reserved.