625 Alloy

Alloy name: 625
Diagram No.: 1113
Type of diagram: TTT
Chemical composition in weight %: 21.28% Cr, 8.7% Mo, 3.83% Fe, 3.58% Nb, 0.27% Mn, 0.30% Si, 0.28% Ti, 0.029% C, 0.007% Ta, <0.005% P, <0.002% S, balance is Ni
Alloy group: Nickel-based alloys
Note: TTT diagram of the Gamma’’ and Delta phases in the studied Alloy 625.
The TTT diagram for the Delta and the Gamma’’ precipitation established from high resolution SEM observations of all the investigated thermal exposures is presented in Fig. The Delta phase is observed to precipitate in the 650°C-900°C temperature domain and preferentially between 700°C and 800°C, while the Gamma’’ phase was found to precipitate in the 550°C-750°C temperature domain, with a preferential formation at 650°C and 700°C. These precipitation domains are in quite good agreement with data extracted from the open literature [2, 11, 12, 14]. Some differences in the Delta precipitation nose were however noted between the present study and other studies, see e.g. [22].
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.


Copyright © 2019 by Steel Data. All Rights Reserved.