Synthetic Slag

Name: Synthetic Slag
Diagram No.: 1121
Type of diagram: TTT
Chemical composition in weight %: See the table
Group: Slags
Note: TTT diagram for the onset of crystallization of sample 1.
Three slag samples were studied and their compositions are listed in table. The liquidus temperature (TL) and the eutectic temperature (TEUT) were determined from the phase diagrams for the present slag systems. It is well known from classical nucleation theory that the onset of crystallization in slags must be a function of cooling rate. To determine the transformation kinetics of crystallization behavior in an undercooled slag one must construct either time temperature transformation (TTT) or continuous cooling transformation (CCT) curves. Figure shows a TTT diagram obtained by the DHTT for the onset crystallization for sample 1. The obtained TTT curve forms a classic C-shape as predicted by classical crystal growth and nucleation theory with the nose position at 1100C with a minimum incubation time of 60 seconds.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.