Western Coal Slag
Name: Western Coal Slag
Diagram No.: 1127
Type of diagram: TTT
Chemical composition in weight %: See the table
Group: Slags
Note: TTT diagram for crystal precipitation in western coal slag under CO/CO2 = 1.8.
Fig. shows the TTT diagram of the crystallization of western coal slag. Crystals precipitated very fast at all the temperatures examined. This result showed that when the viscosity was measured, the melt was in fact a mixture of liquid slag and crystals. Although the TTT curve seemed to have two “noses”, the crystalline phase found at the two nose-temperatures had no difference. In the temperature range of 1200~1500ºC, the only crystalline phase predicted and observed while obtaining TTT diagram was MgAl2O4 spinel.
Reference: Not shown in this demo version.
Transformation Diagram
Price: 30.00 US $
Buy Online Transformation Diagram
Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys
Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.