CSAM (CaO, SiO2, Al2O3, MgO) Slags

Name: CSAM (CaO, SiO2, Al2O3, MgO)
Diagram No.: 1163
Type of diagram: CCT
Chemical composition in weight %: See the table
Group: Slags
Note: CCT Diagram for slag samples with (a) NBO/T = 1.44 (b) NBO/T = 1.56 (c) NBO/T = 1.71(d) NBO/T = 1.78 (e) NBO/T = 1.94 (f) Comparison of all CCT diagrams.
The CCT diagrams of the slag were obtained by continuously cooling the samples at different rates and recording the start time of the crystallization. The CCT diagrams for the five slag compositions (NBO/T=1.44-1.94) are presented in Figure 1 (a)(e). The slag with NBO/T<1.44 did not crystalize when cooled even as slow as 0.2 C.s-1. The summary of all CCT diagrams is shown in Figure 1 (f) for comparison.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.





Copyright © 2019 by Steel Data. All Rights Reserved.