CaO-Al2O3-Based Slag

Name: CaO-Al2O3-Based Slag
Diagram No.: 1171
Type of diagram: CCT
Chemical composition in weight %: See the table
Group: Slags
Note: Non-isothermal CCT diagram for the calcium-aluminate-based slags containing 2.5, 5 and 7.5 wt pct MgO at a CaO/Al2O3 ratio of 1.0.
The CCT diagrams of the CaO-Al2O3-based slag with 2.5, 5 and 7.5 wt pct MgO and a constant CaO/Al2O3 ratio of 1 are shown in Figure 5 for cooling rates of 25, 50, 100, 400, and 800 K/minutes, initiated from 1843 K (1570 C). The results showed that higher concentrations of MgO increased the crystallization starting temperature when the cooling rates were not more than 100 K/minutes. For cooling rates of 400 K/minutes and above with 5.0 and 7.5 wt pct MgO, increased MgO addition to the slag had relatively little effect, while no crystal phase was observed for 2.5 wt pct MgO.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.



Copyright © 2019 by Steel Data. All Rights Reserved.