7085-T6 Alloy

Alloy name: 7085-T6
Diagram No.: 1182
Type of diagram: TTP
Chemical composition in weight %: max. 0.04% Cr, 1.30-2.00% Cu, max. 0.08% Fe, 1.20-1.80% Mg, max. 0.04% Mn, max. 0.06% Si, max. 0.06% Ti, 7.00-8.00% Zn, 0.08-0.15% Zr, balance is Al
Alloy group: Aluminium-based alloys
Note: Figure is another example of a TTP diagram for two properties. This time solute loss is measured by yield strength, the effect of grain boundary precipitate is measured by toughness. For quench interrupted 3OU Có35O C, only at short time is needed for precipitates to weaken the grain-boundary enough for toughness to drop nearly in half. At longer hold times, when solute depletion becomes significant, the matrix becomes more ductile, and the toughness actually increases. A survey of all available TTP diagrams for toughness found this pattern to be general.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.




Copyright © 2019 by Steel Data. All Rights Reserved.