U10Mo Alloy

Alloy name: U10Mo
Diagram No.: 1203
Type of diagram: TTT
Chemical composition in weight %: 10% Mo, balance is U
Alloy group: Uranium-based alloys
Note: Figure shows the TTT diagram of U-10Mo with various Zr compositions, 0.0, 1.0, 2.0, 4.0, and 6.0 wt.% Zr, presented by Peterson et al. [27].
Higher Zr composition pushes the nose of the TTT diagram to shorter times. With only a 6 wt.% Zr content, the reaction nucleates after around 3 minutes at 560 C, the HIPing temperature. With 10 and 20 wt.% Zr, and assuming the observed trend continues, one can then assume almost instantaneous reaction. As seen from the difference in time to 100% transformation between the U10Mo and U10Mo1Zr samples, higher Zr content would also promote the completion of the reaction. Unfortunately there is no data on the specific change in reaction order in higher Zr content alloys.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.



Copyright © 2019 by Steel Data. All Rights Reserved.