Cu-Be Alloy

Alloy name: Cu-Be
Diagram No.: 145
Type of diagram: TTT
Chemical composition in weight %: a.) 1.5% Be, balance is Cu. b.) 2% Be, balance is Cu. c.) 1.8% Be, 0.2% Co, balance is Cu.
Alloy group: Copper-based alloys
Note: Undeformed specimens. Treatment: Solution treated at 800C (1472 F) for 20 min under argon and quenched in iced water, then aged from 200-500C (392-932 F) for 10 to 106 s. An oil bath was used for aging at 200 and 250C (392 and 482 F), and salt mixtures of NaNO2 and NaNO3 for aging over the temperature region from 300 to 500C (572 to 932 F).
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.