Cu-Zn Alloy

Alloy name: Cu-Zn
Diagram No.: 157
Type of diagram: TTT
Chemical composition in weight %: 40.5% Zn, balance is Cu
Alloy group: Copper-based alloys
Note: Treatment: Specimens were held within 5 deg. at 880C (l526F) for 2 min in a vertical furnace containing an atmosphere of nitrogen, 3% hydrogen and zinc vapor, then quenched into 10% aqueous sodium hydroxide at 0C. The quenched structure was entirely metastable beta-prime phase with a grain size of 1-2 mm. Subsequent heat-treatment in the range 150-350 C (802662F} was in a nitrate-nitrite bath, and above 850C (662F) in a lead bath controlled to within 3 deg.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.