Mg-Mn Alloy

Alloy name: Mg-Mn
Diagram No.: 167
Type of diagram: TTP
Chemical composition in weight %: 1.58% Mn, balance is Mg
Alloy group: Magnesium-based alloys
Note: Time-temperature-precipitation diagram. The precipitation of Mn is a rapid transformation, starting after only 7 s and being complete after 10 min aging at 500C (932F). Treatment: Samples were aged at temperatures between 390 and 530C (734 and 986F) in a salt bath furnace and subsequently water quenched. The bath temperature was controlled within 2 deg.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.







Copyright © 2019 by Steel Data. All Rights Reserved.