Ni-Al-Mo-W-C Alloy

Alloy name: Ni-Al-Mo-W-C
Diagram No.: 175
Type of diagram: TTP
Chemical composition in weight %: 6.8% Al, 14.4% Mo, 6.1% W, 0.04% C, balance is Ni
Alloy group: Nickel-based alloys
Note: Treatment: Materials were prepared from rapidly solidified powders. Stainless steel cans were filled with powder, sealed, outgassed, and extruded at a temperature just below the gamma prime solvus. Slices 1 to 2 mm thick were cut from the as-extruded bars and sealed in quarts in vacuum. Specimens were cycled twice above and then below the gamma prime solvus before being exposed at 3092 C (1700 F) for 500 h and air cooled.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.