Rene 41 Alloy

Alloy name: Rene 41
Diagram No.: 189
Type of diagram: TTP
Chemical composition in weight %: 0.08% C, 19.31% Cr, 10.02% Co, 9.11% Mo, 3.23% Ti, 1.51% Al, 0.000% B, 2.34% Fe, balance is Ni
Alloy group: Nickel-based alloys
Note: Treatment: Solution treated at 1177 C (2150 F), aged in air at 760 to 1093 C (1400 to 2000 F) at 38 C (100 F) intervals for 5000 h, and at 1149°C (2100°F) for 2000 h.
Reference: IKE. Collins, “Relative Long-Time Stability of Carbide and Intermetallic Phaeer in Nickel-Baee Superalloys,” Trans. ASM, Vol 62, 1969, pp. 82-104.

Transformation Diagram


Click the image to enlarge the diagram.

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.