Nimonic PE16 Alloy

Alloy name: Nimonic PE16
Diagram No.: 218
Type of diagram: TTP
Chemical composition in weight %: 17.1% Cr, 42.5% Ni, 3.1% Mo, 1.2% Ti, 1.3% Al, 0.03% Zr, 0.05% Mn, 0.0003% B, 0.06% C, balance is Ni
Alloy group: Nickel-based alloys
Note: Treatment: Specimenr were rapidly heated to 1100C (2012 F) and maintained at temperature for 1 h, then rapidly cooled to an aging temperature between 625 and 950C (1157 and 1742 F) and maintained at the desired aging temperature for times varying between 15 and 3600 s, followed by rapid cooling to ambient temperature.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.






Copyright © 2019 by Steel Data. All Rights Reserved.