Nicrofer 4320 Ti Alloy

Alloy name: Nicrofer 4320 Ti Alloy
Diagram No.: 234
Type of diagram: TTS
Mat. No. (Wr. Nr.) designation: 2.4852
DIN designation: NiCr20FeMo3TiCuAl
UNS designation: N09925
Chemical composition in weight %: 0.03% C, 1.00% Mn, 0.50% Si, 0.03% S, 0.03% P, 42.00-46.00% Ni, 19.50-22.50% Cr, 22.0% Fe, 2.50-3.50% Mo, 1.50-3.0% Cu, 1.90-2.40% Ti, 0.10-0.50% Al, 0.50% Nb
Note: Time-temperature-transformation diagram for solution annealed Nicrofer 4320 Ti material.
Reference: Not shown in this demo version.
Alloy group: Nickel-based alloys

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.






Copyright © 2019 by Steel Data. All Rights Reserved.