Cast Alloy 718 Alloy

Alloy name: Cast Alloy 718
Diagram No.: 260
Type of diagram: TTP
Chemical composition in weight %: No data
Alloy group: Nickel-based alloys
Note: Treatment: Aged at 649 to 1093 C (1200 to 2000 F).
Reference: R.G. Carlson, J.F. Radavich, "Microstructural Characterization of Cast 718," Superalloy 718 - Metallurgy and Applications, E.A. Loria, ed., TMS, 1989, pp. 79-96.

Transformation Diagram


Click the image to enlarge the diagram.

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.