Alloy 718 Alloy

Alloy name: Alloy 718
Diagram No.: 271
Type of diagram: CCT
Chemical composition in weight %: 19.9% Fe, 18.2% Cr, 6.1% Nb, 2.9% Mo, 1.16% Ti, 0.2% Mn, balance is Ni
Alloy group: Nickel-based alloys
Note: Treatment: Cylinders 40 mm long x 10 mm diam were vacuum sealed in quartz and homogenized at 1180 C (2166 F) for 24 h, water quenched. Dilatometer specimens were machined from the cylinders. The dilatometer specimens were heated to 1180 C (2166 F) at 0.6 C/s, held for 30 min and then cooled at various rates. Companion specimens were treated identically but water quenched from different temperatures and examined metallographically.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.