Single Crystal Alloy 800

Alloy name: Single Crystal Alloy 800
Diagram No.: 322
Type of diagram: TTP
Chemical composition in weight %:
Composition: 8.0% Cr, 7.5% Co, 1.6% Mo, 4.0% W, 5.0% Ta, 1.5% Ti, 6.8% Al, 3.0% Re, balance is Ni
1% Re composition: 7.5% Cr, 5.0% Co, 2.0% Mo, 3.0% W, 12.0% Ta, 1.0% Ti, 5.0% Al, 1.0% Re, balance is Ni
2% Re composition: 7.5% Cr, 6.0% Co, 2.0% Mo, 2.0% W, 12.0% Ta, 1.0% Ti, 5.0% Al, 2.0% Re, balance is Ni
3% Re comporition: 7.5% Cr, 5.0% Co, 2.0% Mo, 1.0% W, 12.0% Ta, 1.0% Ti, 6.0% Al, 3.0% Re, balance is Ni
4% Re composition: 7.5% Cr, 5.0% Co, 2.0% Mo, 12.0% Ta, 1.0% Ti, 5.0% Al, 4.0% Re, balance is Ni
Alloy group: Nickel-based alloys
Note: Treatment: Fully solutioned and aged specimens were exposed at 871,982, 1093, 1149, and 1204 C (1600, 1800, 2000, 2100 and 22OO F) for times up to 1000 h to determine the occurrence of topologically close packed (TCP) phases.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.