8090 Alloy

Alloy name: 8090
Diagram No.: 37
Type of diagram: TTP
Chemical composition in weight %: 2.28% Li, 0.86% Cu, 0.90% Mg, 0.13% Zr, 0.13% Fe, 0.06% Si, balance is Al
Alloy group: Aluminium-based alloys
Note: No data
Reference: G.M. Colvin, E.A. Starke, Jr., SAMPE Q., July 1988, Vol 19, No. 4, pp. 10-21, as published in Aerospace Structural Handbook for Nonferrous Alloys, June 1990.

Transformation Diagram


Click the image to enlarge the diagram.

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.