Al - 22 at.% Zn - 0.1 at.% Sn Alloy

Alloy name: Al - 22 at.% Zn - 0.1 at.% Sn
Diagram No.: 4
Type of diagram: TTP
Chemical composition in atomic %: 22 at.% Zn, 0.1 at.% Sn, balance is Al
Alloy group: Aluminum-based alloys
Note: Specimen were homogenired in air at 400C (752 F) for approx. 30 min and then quenched into a water or oil bath located directly beneath the homogeniration furnace. Isothermal aging was accomplished in a silicone oil bath controlled to with 1 deg over the temperature range 60 to 240 C (122 to 464 F). Room temperature aging was carried out in an insulated oil bath and a OC (320 F) aging treatment water.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.







Copyright © 2019 by Steel Data. All Rights Reserved.