Ti-Mo Alloy

Alloy name: Ti-Mo
Diagram No.: 450
Type of diagram: CCT
Chemical composition in weight %: 4.57% Mo, balance is Ti
Alloy group: Titanium-based alloys
Note: Treatment: Sponge titanium with a Brine11 hardness of 112-116, prepared by an argon-arc furnace, hot rolled into sheets, surface cleaned and homogenised at 900 C (1652°F) for 20 days.
Reference: Y.C. Huang, S. Sucuki, H. Kaneko, T. Sato, “Continuous Cooling-Transformation of Beta-Phase in Binary Titanium Alloys,” proceedings of an International Conference held at the Royal Festival Hall, London, 21-24 May, lQ68, The Science, Technology and Application of Titanium, RI. Jaffee, N.E. Promisel, Eds., Pergamon Press, Oxford, 1970, pp. 695-698.

Transformation Diagram


Click the image to enlarge the diagram.

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.