Ti-6248 Alloy

Alloy name: Ti-6248
Diagram No.: 497
Type of diagram: CCT
Chemical composition in weight %: 5.9% Al, 1.99% Sn, 3.90% Zr, 7.96% Mo, 0.076% Fe, 0.004% H, 0.124% 0, balance is Ti
Alloy group: Titanium-based alloys
Note: Treatment: Solution annealed at 1020°C (1870°F) for 20 min.
Reference: W.W. Cias, “Phase Transformation Kinetics, Microstructures, and Hardenability of the Ti-6Al-2Sn-4Zr-8Mo Titanium Alloy,” Rp-27-72-07, Climax Molybdenum, 25 October 1972.

Transformation Diagram


Click the image to enlarge the diagram.

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.