Zr-Mo Alloy

Alloy name: Zr-Mo
Diagram No.: 561
Type of diagram: TTT
Chemical composition in weight %: 7.5% Mo, balance is Zr
Alloy group: Zirconium-based alloys
Note: Treatment: Forged alloy rods were held at 975 to 1000C (1787 to 1832 F) for 15 to 20 min, isothermally quenched, held for a given length of time, then rapidly water quenched.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.









Copyright © 2019 by Steel Data. All Rights Reserved.