Ti6Al4V Alloy

Alloy name: Ti6Al4V
Diagram No.: 599
Type of diagram: TTT
Chemical composition in weight %: 6.00% Al, 3.99% V, 0.25% Fe, 0.20% O, 0.02% C, 0.01% N, balance is Ti
Alloy group: Titanium-based alloys
Note: Modeled (single transformation curve) and JMatPro calculated TTT diagram for grain boundary and intragranular nucleation and growth. The microstructure model seeks to describe the evolution of alpha phase fraction with temperature. Ti-6Al-4V is a two phase, alpha (HCP) + beta (BCC), at room temperature. Above approximately 1273K (beta transus tempertaure) the beta phase is stable.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.






Copyright © 2019 by Steel Data. All Rights Reserved.