Ti–52Ni Alloy

Alloy name: Ti–52Ni
Diagram No.: 609
Type of diagram: TTT
Chemical composition in atomic %: 52.5 at.% Ni, balance is Ti
Alloy group: Titanium-based alloys
Note: In fact these transformations are summarized by TTT (time–temperature–transformation) diagram as shown in Fig. The TTT diagram also shows the upper temperature limit for each precipitate, e.g. the upper limit for the Ti3Ni4 phase is 680 C. Kainuma et al. carried out a similar work for the Ti–54Ni and Ti–56Ni alloys in addition to the Ti–52Ni alloy, and determined the TTT diagrams for these alloys. They also determined the solubility limit of the TiNi phase on Ni-rich side, and confirmed that the solubility limit by Wasilewski et al. was correct.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.





Copyright © 2019 by Steel Data. All Rights Reserved.