Zn-Al Alloy

Alloy name: Zn-Al
Diagram No.: 613
Type of diagram: TTT
Chemical composition in weight %: 18% Al, 0.87% Cu, 0.037% Mg, 0.024% Ca, balance is Zn
Alloy group: Zinc-based alloys
Note: TTT curves for the eutectoid transformation of 18 pct A1 alloy sulution treated at 350°C.
Reference: FU—WEN LING AND DAVID E.LAUGHLIN, The Kinetics of Transformation in Zn-Al Superplastic Alloys, METALLURGICAL TRANSACTIONS A, Volume 10A, July 1979, pp. 921-928.

Transformation Diagram


Click the image to enlarge the diagram.

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.