Bi1.7 Pb0.4 Sr1.6 Ca2.4 Cu3.6 Ox Alloy

Alloy name: Bi1.7 Pb0.4 Sr1.6 Ca2.4 Cu3.6 Ox
Diagram No.: 632
Type of diagram: TTT
Chemical composition in weight %: Bi 1.7Pb 0.4 Sr1.6 Ca2.4 Cu3.6 Ox.
Alloy group: Bismuth-based alloys
Note: TTT diagram in the solidification of the melt with a composition of Bi1.7 Pb0.4 Sr1.6 Ca2.4 Cu3.6 Ox.
Phase changes during the solidification of Bi-Pb-Sr-Ca-Cu-O melt were studied. Under solidification processes with constant cooling rates of 0.001-10 C/s, Bi2Sr2Ca2Cu3Ox(2223) is not formed but Bi2Sr2Ca2Cu3Ox(2212) and Bi2Sr2CuOx(2201) are observed. The time-temperature-transformation (TTT) diagram in the solidification of the melt is proposed based on the results of X-ray diffraction (XRD) analysis. A high-Tc superconductor phase of 2223 is formed through the isothermal treatment at 850 C for above 150 ks.The analyses of XRD and scanning electron micrograph (SEM) with energy dispersive X-ray (EDX) suggest that 2201 needles are crystallized at the interface between (Ca,Sr)2CuO3 crystals and melt, and the part of 2201 crystals transforms to 2212 and 2223 crystals by the diffusion of Ca, Sr, and Cu ions.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.


Copyright © 2019 by Steel Data. All Rights Reserved.