Ti-6554 Alloy

Alloy name: Ti-6554
Diagram No.: 635
Type of diagram: TTT
Chemical composition in weight %: Ti-6Cr-5Mo-5V-4Al alloy (Ti-6554): 5.7% Cr, 4.7% Mo, 4.81% V, 3.93% Al, 0.08% Fe, 0.028% Si, 0.025% V, balance is Ti
Alloy group: Titanium-based alloys
Note: TTT curve of Ti-6554 alloy. Metallographic method was used for the determination of TTT curve of Ti-6554 titanium alloy. The results show that the 'nose'temperature of isothermal transformation is about 540 C. When the alloy is aged at 540 C, alpha phase precipitates fastest, and only 5 min is needed. Moreover, this alloy has fast aging response. When the alloy is aged at 480-600 C, the beginning time of alpha phase precipitated from metastable beta phase is less than 30 min.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.





Copyright © 2019 by Steel Data. All Rights Reserved.