Cu-Ti Alloy

Alloy name: Cu-Ti
Diagram No.: 637
Type of diagram: TTT
Chemical composition in weight %: 3% Ti, balance is Cu
Alloy group: Copper-based alloys
Note: Preliminary data on the kinetics of the cellular precipitation were obtained by quantitative metallographic analyses. The amount of cellular precipitation increases with aging time at 450°C. The TTT diagram of the cellular precipitation was constructed as presented in Figure 6. It is obvious that the TTT diagram in the range of temperature studied is the portion below the “nose” of the normal TTT curve.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.







Copyright © 2019 by Steel Data. All Rights Reserved.