Al-300 ppm Fe Alloy

Alloy name: Al-300 ppm Fe
Diagram No.: 656
Type of diagram: TTP
Chemical composition in weight %: 299 ppm Fe, 2 ppm Si, 1 ppm Cu, 1 ppm Mn, 0 ppm Cr, 1 ppm Ni, 1 ppm Zn, 1 ppm Ga, 0.3 ppm Ti, balance is Al
Alloy group: Aluminim-based alloys
Note: TTP diagrams of the undeformed (broken curve) and 65% colddrawn (solid curves) specimens. Solid circle C shows the aging condition for TEM observation in which Al3Fe phase precipitates were observed, while open circles A and B show the aging condition for TEM, respectively.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.







Copyright © 2019 by Steel Data. All Rights Reserved.