U-Mo Alloy

Alloy name: U-Mo
Diagram No.: 659
Type of diagram: TTT
Chemical composition in weight %: 5.4% Mo, 8% Mo, 10% Mo, 12% Mo, balance is U
Alloy group: Uranium-based alloys
Note: TTT diagrams illustrating initial resistivity decrease for U-Mo alloys from R. J. VAN THYNE and D. J. Mc PHERSON.
Reference: G. BEGHI, GAMMA PHASE URANIUM-MOLYBDENUM FUEL ALLOYS, EUROPEAN ATOMIC ENERGY COMMUNITY EURATOM, EUR 4-O53 e, 1968, 49, pp. 1-80.

Transformation Diagram


Click the image to enlarge the diagram.

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.