6082 Alloy

Alloy name: 6082
Diagram No.: 669
Type of diagram: CCT
Chemical composition in weight %: <0.2% Zn, 0.6—1.2% Mg, <0.10% Cu, 0.40—1.0% Mn, 0.25% Cr, <0.1% Ti, <0.50% Fe, 0.7-1.2% Si, balance is Al
Alloy group: Aluminium-based alloys
Note: CCT diagram of 6082 aluminum alloy (holding at 550 C for 1 h).
Electrical resistance–temperature curves of 6082 aluminum alloy at various cooling rates during continuous cooling was obtained by in–situ resistance measurement. Phase transformation start and finish temperatures were ascertained by the slope change of resistance–temperature curves. Continuous cooling transformation (CCT) diagram for 6082 aluminum alloy was plotted. The phase transformation start and finish temperature decreases with the increase of cooling rates when the cool- ing rate is slow, but as the cooling rate increases to a certain rate the phase transformation start temperature increases suddenly and then decreases continously. Phase transformations mainly take place between 220 and 400 C. Critical cooling rate for preventing phase transformation is between 16—34 C/s. For plates 20 mm in thickness is proper to quench by 60 C water.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.