Nimonic 263 Alloy

Alloy name: Nimonic 263
Diagram No.: 676
Type of diagram: CCT
Chemical composition in weight %: 0.06% C, 19.60% Co, 20.1% Cr, 6.00% Mo, 2.00% Ti, 0.4% Al, 0.001% Cu, 0.0013% O, 0.006% N, balance is Ni
Alloy group: Nickel-based alloys
Note: TTT diagram of Ni-263
Reference: V. Acharya, S. Ramesh and G.V.S. Murthy, Characterization of Intermetallic Precipitates in Ni-Base Alloys by Non-destructive Techniques, Intech, Chapter 11 from the book Superalloys, 2015, https://www.intechopen.com/books/superalloys, pp. 1-29.

Transformation Diagram


Click the image to enlarge the diagram.

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.