Ni2Cr Alloy

Alloy name: Ni2Cr
Diagram No.: 684
Type of diagram: TTT
Chemical composition in weight %: Ni2Cr
Alloy group: Nickel-based alloys
Note: (Color online) Calculated Isothermal TTT diagram (solid circles) for a fcc-based matrix of a binary Ni2Cr alloy transforming into the oP6-ordered phase, with transformation rate of 10%. The experimentally deduced TTT diagram (solid squares) [7] for the same transformation rate is also shown for comparison.
The location of the nose of the experimental TTT curve has been used to determine the kinetic parameters that are defined below in the MOB database for subsequent calculations. The detailed results of the simulations for a 10% transformation are reported in the TTT curve displayed in Fig. 4. The shape of this C curve is detailed in Table 1 and by the curves displayed in Fig. that show the fraction of oP6-phase formed in the fcc matrix versus time at various temperatures.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.



Copyright © 2019 by Steel Data. All Rights Reserved.