Zr41.2Ti13.8Cu12.5Ni10.0Be22.5 Glass

Name: Zr41.2Ti13.8Cu12.5Ni10.0Be22.5
Diagram No.: 702
Type of diagram: TTT
Chemical composition in weight %: Zr41.2Ti13.8Cu12.5Ni10.0Be22.5
Alloy group: Zirconium-based glass
Note: Time–temperature-transformation diagram reflecting the onset of crystallization as a function of undercooling (black point). Below 800 K two crystallization events are observed. The primary crystallization (point with cross) is followed by secondary crystallization (black pont).
Reference: Y. J. Kim, et al., Experimental determination of a time–temperature-transformation diagram of the undercooled Zr41.2Ti13.8Cu12.5Ni10.0Be22.5 alloy using the containerless electrostatic levitation processing technique, Appl. Phys. Lett. 68 (8), 19 February 1996, pp. 1057-1059.

Transformation Diagram


Click the image to enlarge the diagram.

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.