AW-7921-T4 Alloy

Alloy name: AW-7921-T4
Diagram No.: 704
Type of diagram: CCT
Chemical composition in weight %: 0.11% Si, 0.24% Fe, 0.13% Cu, 0.06% Mn, 2.63% Mg, 7.28% Zn, 0.01% Ni, 0.02% Cu, 0.05% Ti, 0.11% Zr, balance is Al
Alloy group: Aluminium-based alloys
Note: Simulated CCT diagram of AA 7921. Precipitation during cooling is generally described by continuous cooling transformation (CCT) diagram. A simulated CCT diagram for 0.5% transformation fraction using JMATPRO software is shown in Figure. In this CCT diagram it is shown that the precipitation of stable ni-phase (MGZN2) and T-phase (T-ALCUMGZN) has finished around 200.C.Therefore, at cooling rates >5 K s(-1) the precipitation of these two phases will be suppressed.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.





Copyright © 2019 by Steel Data. All Rights Reserved.