Ti-10V-2Fe-3Al, Beta C, Ti-15-3-3-3, Ti-5553, Beta21S Alloys

Alloy name: Ti-10V-2Fe-3Al, Beta C, Ti-15-3-3-3, Ti-5553, Beta21S
Diagram No.: 711
Type of diagram: TTT
Chemical composition in weight %:
Ti-10V-2Fe-3Al: 10V2Fe3Al
Ti-5553: 5Al5V5Mo3Cr0.5Fe
Ti-15V-3Al-3Sn-3Cr: 15V3Cr3Al3Sn
Beta 21S: 15Mo2.7Nb3Al0.2Si
Beta C: 3Al8V6Cr4Mo4Zr
Alloy C: 35V15Cr
Alloy group: Titanium-based alloys
Note: TTT C-curves for initial a precipitation (lower-temperature metastable phase reactions are omitted for clarity) in selected beta titanium alloys following quenching from respective solution treatment temperatures. Note that Ti-5553 and Ti-10V-2Fe-3Al are subtransus solution treated while the other alloys are supertransus solution treated prior to quenching.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.