60-40 Alpha-Beta Brass Alloy

Alloy name: 60-40 Alpha-Beta Brass
Diagram No.: 722
Type of diagram: TTT
Chemical composition in weight %: 60-40 Alpha-Beta Brass
Alloy group: Copper-based alloys
Note: TTT CURVES FOR A 60-40 Alpha-Beta Brass (Adapted from Flewitt and Towner). Time-Temperature Transformation (TTT) curves for a 60-40 brass. The separate "C"-Curves are indicative of a proeutectoid reaction at high temperatures, and a bainitic reaction at lower temperatures. (Adapted from Flewitt and Towner). The overall similarity in structure, morphology and kinetics between the intermediate temperature transformation products in the brasses, the binary Cu-Al alloy and the NABs, strongly suggests that bainite is formed in all three aiioy systems.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.





Copyright © 2019 by Steel Data. All Rights Reserved.