Cu-11.8% Al Alloy

Alloy name: Cu-11.8% Al
Diagram No.: 723
Type of diagram: CCT
Chemical composition in weight %: 11.8% Al, balance is Cu
Alloy group: Copper-based alloys
Note: Microstructure map and CCT curves for a Cu-11.8% Al alloy. Solution treated at 900C for i hr. Adapted from Brezina 1982. Microstructure map (a) and Continuous-Cooling-Transformation (CCT) Curves (b) for a eutectoidal Cu-Al alloy. Cooling rates and times (experimentally determined) were converted to equivalent bar thicknesses in a given cooling medium, using standard thermal data. Both the map, and the CCT curves relate to the center of the bar. (Adapted from Brezina). The CCT curves and the microstructure maps are both "read" from "top to bottom". Reasonable agreement is seen between the CCT curves of Brezina [this figure] and the TTT curves which were presented in Figure. Note that alpha* denotes a mixture of martensite and bainite.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.



Copyright © 2019 by Steel Data. All Rights Reserved.