BOF Slag

Name: BOF Slag
Diagram No.: 759
Type of diagram: TTT
Chemical composition in weight %: Original slag: 44.5% CaO, 20.6% Fe (total iron in the oxides), 10.2% Fe2+, 10.4% Fe3+, 10.14% SiO2, 4.78% MnO, 2.18% MgO, 2.05% Al2O3, 2.43% P2O5, 0.89% TiO2, 0.37% V2O5
Group: Slags
Note: TTT diagram of the original and modified BOF slags. 5 A, 10 A, and 15 A indicate the 5, 10, and 15 wt% Al2O3 modified BOF slags, respectively. Tn1, Tn2, Tn3, and Tn4 are the nose temperature of original, 5 A, 10 A and 15 A slags. The line is drawn as a guide for reading.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.






Copyright © 2019 by Steel Data. All Rights Reserved.