Pb-0.06% Ca, Pb-0.08% Ca, Pb-0.10% Ca Alloys

Alloy name: Pb-0.06% Ca, Pb-0.08% Ca, Pb-0.10% Ca
Diagram No.: 777
Type of diagram: TTT
Chemical composition in weight %:
0.06% Ca, balance is Pb
0.08% Ca, balance is Pb
0.10% Ca, balance is Pb
Alloy group: Lead-based alloys
Note: TTT diagram for the concentrations of calcium of 600, 800 and 1000 ppm. Samples were cast, then cooled in liquid state at aminimum of 40 C/s to -196 C. Curves are obtained by resistivity and hardness measurements performed in a subsequent in situ heat treatments carriedout in the temperature range -20 C to 180 C. The solid lines through the data points are curve fits.
Additional links: No. 775, No. 776, No. 777, No. 778, No. 779, No. 780
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service
Transformation Diagrams of Non-Ferrous Alloys

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.



Copyright © 2019 by Steel Data. All Rights Reserved.